Laser-induced damage of high reflectors for Ti:sapphire laser system

Not Accessible

Your library or personal account may give you access

Abstract

A broadband (~176 nm, R>98%, 'lambda'0=800 nm) and high laser-induced damage threshold (LIDT=2.4J/cm2) TiO2/HfO2/SiO2 high reflector (HR) for Ti:sapphire chirped-pulse amplification (CPA) laser system is fabricated by the electron beam evaporation. The refractive index and extinction coefficient of TiO2 and HfO2 films are calculated from single-layer films' transmittance spectra. The properties of HR are mainly determined by the high refractive index material. The high refractive index leads to wide bandwidth. A low extinction coefficient indicates low absorption and high LIDT. The possible damage mechanism of HR is discussed.

© 2007 Chinese Optics Letters

PDF Article
More Like This
Comparison of femtosecond and nanosecond laser-induced damage in HfO2 single-layer film and HfO2-SiO2 high reflector

Lei Yuan, Yuanan Zhao, Guangqiang Shang, Chengren Wang, Hongbo He, Jianda Shao, and Zhengxiu Fan
J. Opt. Soc. Am. B 24(3) 538-543 (2007)

Effect of nanosecond laser pre-irradiation on the femtosecond laser-induced damage of Ta2O5/SiO2high reflector

Shunli Chen, Yuan’an Zhao, Dawei Li, Hongbo He, and Jianda Shao
Appl. Opt. 51(10) 1495-1502 (2012)

Cited By

You do not have subscription access to this journal. Cited by links are available to subscribers only. You may subscribe either as an Optica member, or as an authorized user of your institution.

Contact your librarian or system administrator
or
Login to access Optica Member Subscription

Select as filters


Select Topics Cancel
© Copyright 2024 | Optica Publishing Group. All rights reserved, including rights for text and data mining and training of artificial technologies or similar technologies.