Abstract
Optically transparent Er3+-doped tellurite-based nanocrystallized glasses with the composition of 70TeO2-15Li2O-15Nb2O5-0.5Er2O3 (mol) have been prepared by a conventional melting quenching and the subsequent heat treatment processes. The sizes of grown nanocrystals in glass matrix appear to be 35-50 nm from the X-ray diffraction (XRD) measurement. The microhardness measurement shows that the Vickers hardness values of the nanocrystallized tellurite glasses are larger (33%-62%) than those in the base glass. The Raman spectra imply that the maximum phonon energy of the based glass decreases and shifts from 668 to 638 /cm after heat-treatment. Visible upconversion luminescence and infrared luminescence of the base glass and heat-treated glasses under 980-nm laser diode (LD) excitation are investigated. The 524-, 546- and 656-nm upconversion intensities by 980-nm pumping increase significantly.
© 2005 Chinese Optics Letters
PDF Article
More Like This
Cited By
You do not have subscription access to this journal. Cited by links are available to subscribers only. You may subscribe either as an Optica member, or as an authorized user of your institution.
Contact your librarian or system administrator
or
Login to access Optica Member Subscription