Abstract

Fabrication technology of the Yb^(3+):Er^(3+) co-doped glass samples is introduced. Photoluminescence (PL) characteristics of a single sample were experimentally investigated. The PL peak intensities of two samples in series were measured and discussed. The results show that the PL peak intensities of two samples in series depend on pump manners and arrangement of the samples. The better amplification ability can be obtained by two samples in series doped with low-concentration ytterbium instead of a single sample doped with high-concentration ytterbium.

© 2005 Chinese Optics Letters

PDF Article

References

You do not have subscription access to this journal. Citation lists with outbound citation links are available to subscribers only. You may subscribe either as an OSA member, or as an authorized user of your institution.

Contact your librarian or system administrator
or
Login to access OSA Member Subscription

Cited By

You do not have subscription access to this journal. Cited by links are available to subscribers only. You may subscribe either as an OSA member, or as an authorized user of your institution.

Contact your librarian or system administrator
or
Login to access OSA Member Subscription