Abstract
Herein, the dependence of the dispersed phase diameter on the shear history during melt processing is verified experimentally. We fabricated different kinds of poly(methyl methacrylate) (PMMA)/poly(ethylene terephthalate) (PET) blends by modifying the shear rate and shear time in a torque rheometer. Light-scattering sheets (LSSs) were then prepared by compression molding with the above blends. The total transmittance of the LSS with a shear history of 8 min at 30 rpm and then 20 min at 5 rpm achieves 84.8% due to the drop coalescence and larger diameters of the PET scatterers in the PMMA matrix, while the total transmittance of a sheet with a shear history at only 30 rpm is just 70.8%. In addition to high total transmittance, the sheet also features high haze (beyond 92.5%) and tiny direct transmittance (less than 5%), which is vital for uniform illumination and glare protection from lasers and light-emitting diodes.
© 2018 Optical Society of America
Full Article | PDF ArticleMore Like This
Xiao Liu, Ying Xiong, Jiabin Shen, and Shaoyun Guo
Opt. Express 23(14) 17793-17804 (2015)
Ping Yi, Ying Xiong, and Shaoyun Guo
Appl. Opt. 54(34) 10000-10008 (2015)
Tse-Chang Li, Cheng-Fang Ho, and Jen-Fin Lin
Appl. Opt. 54(4) 816-827 (2015)