Abstract

Transmission and reflection measurements in the infrared region between 340 and 40 cm−1 are presented for Irtrans 1–6. Measurements have been performed at room temperature and at liquid nitrogen and liquid helium temperatures.

© 1974 Optical Society of America

Full Article  |  PDF Article

References

  • View by:
  • |
  • |
  • |

  1. A. Hadni, J. Claudel, G. Morlot, P. Strimer, Appl. Opt. 7, 161 (1968); Appl. Opt. 7, 1159 (1968).
    [CrossRef] [PubMed]
  2. J. J. Wijnbergen, W. H. Moolenaar, G. de Groot, Proc. 5th Eslab/Esrin Symposium, Noordwijk (1971).
  3. Eastman Kodak Company, Rochester, New York, 14650.
  4. Kodak Pamphlet No. U 71 and Kodak publication U-72-(1971).
  5. Grubb-Parsons, Walkergate, New Castle upon Tyne 6, England.
  6. Infrared Laboratories Inc., P.O. Box 17015, Tucson, Arizona 85710.
  7. Nextel Velvet Coating 401-C10 Black, 3 M Company, St. Paul, Minnesota 55101.
  8. Commercial Plastics, Boekelosestraat 400, Boekelo, The Netherlands.
  9. D. E. McCarthy, Appl. Opt. 2, 591 (1965); Appl. Opt. 4, 317 (1965).
    [CrossRef]
  10. G. M. Ressler, K. D. Möller, Appl. Opt. 5, 877 (1966).
    [PubMed]
  11. C. M. Randall, R. D. Rawcliffe, Appl. Opt. 7, 213 (1968).
    [CrossRef] [PubMed]

1968 (2)

1966 (1)

1965 (1)

Appl. Opt. (4)

Other (7)

J. J. Wijnbergen, W. H. Moolenaar, G. de Groot, Proc. 5th Eslab/Esrin Symposium, Noordwijk (1971).

Eastman Kodak Company, Rochester, New York, 14650.

Kodak Pamphlet No. U 71 and Kodak publication U-72-(1971).

Grubb-Parsons, Walkergate, New Castle upon Tyne 6, England.

Infrared Laboratories Inc., P.O. Box 17015, Tucson, Arizona 85710.

Nextel Velvet Coating 401-C10 Black, 3 M Company, St. Paul, Minnesota 55101.

Commercial Plastics, Boekelosestraat 400, Boekelo, The Netherlands.

Cited By

OSA participates in CrossRef's Cited-By Linking service. Citing articles from OSA journals and other participating publishers are listed here.

Alert me when this article is cited.


Figures (2)

Fig. 1
Fig. 1

Transmission vs wavenumber of Irtrans 1–6 at 295 K (· · · ·), 77 K (– –), and 4.2 K (——).

Fig. 2
Fig. 2

Reflection vs wavenumber of Irtrans 1–6 at 295 K (· · · ·), 77 K (– –), and 4.2 K (——).

Metrics