Abstract
Glass welding by ultrashort laser pulses allows joining without the need of an absorber or a preheating and postheating process. However, cracks generated during the welding process substantially impair the joining strength of the welding seams. In this paper a sample preparation method is described that prevents the formation of cracks. The measured joining strength of samples prepared by this method is substantially higher than previously reported values.
© 2011 Optical Society of America