Abstract

We measured atomic polarization relaxation-time in PDMS coated and uncoated rubidium-loaded hypocycloidal-core Kagome HC-PCF. The measured relaxation-times of 32µs and 24µs in PDMS coated and uncoated fibers are longer two-orders-of-magnitude than the wall-collision-limited relaxation time.