Abstract

We report on experiments carried out with improved pumping schemes and present modeling for further enhancement of direct 8-12 µm generation by self-DFM in Cr:ZnSe laser slabs using a Tm:YLF 1.9-µm pulsed pump source.

© 2006 Optical Society of America