Abstract
Comparing gain in Er-doped tellurite glasses for CO2 absorption measurements, a maximum gain of 2.2dB/cm with 8 ms fluorescence lifetime has been obtained at 1572 nm using a 974 nm pump with intensity of 8kW/cm2.